Batareya shlamining barqarorligi va dispersligi elektrodlar va tayyor akkumulyator mahsulotlarining xususiyatlariga muhim ta'sir ko'rsatadi. Xo'sh, akkumulyator eritmasining barqarorligi va tarqalishini qanday tavsiflash mumkin?
Batareya shlamining barqarorligini tavsiflash usuli
1. Qattiq tarkib usuli
Qattiq tarkibni sinovdan o'tkazish usuli arzon va oson sinov usuli hisoblanadi. Uning printsipi atalani idishga joylashtirish va qattiq tarkibni sinash va tahlil qilish uchun muntazam ravishda bir xil joyda namunalar olishdir. Qattiq tarkibdagi farqni baholab, lityum batareya atalasining barqarorligi cho'kindi, tabaqalanish va boshqa hodisalar mavjudligini aniqlash uchun baholanishi mumkin.
2. Yopishqoqlik usuli
Yopishqoqlikni tekshirish usuli asosan atala barqarorligini aks ettirishi mumkin. Uning printsipi atalani idishga joylashtirish va viskoziteni muntazam ravishda tekshirishdan iborat. Atlamaning barqarorligini yopishqoqlikning o'zgarishi bilan baholash mumkin.
3. Barqarorlik analizatori
Barqarorlik analizatoridan foydalanish ma'lumotlar bilan gaplashishi mumkin. Masalan, Sung va boshqalar. 12 soat ichida birlashtiruvchi sifatida PAA dan foydalangan holda turli pH shlamlarining yorug'lik o'tkazuvchanligi o'zgarishlarini kuzatish uchun barqarorlik analizatoridan foydalangan. Neytral eritmaning dastlabki yorug'lik o'tkazuvchanligi va 12-soatlik o'zgarish qiymatlari kichikroq edi. Uglerod qora materiallari yorug'lik assimilyatsiyasiga ega bo'lganligi sababli, past yorug'lik o'tkazuvchanligi uglerod qora zarralarining yaxshiroq tarqalishini ko'rsatadi va kichikroq mikro-aglomeratlar kattaroq o'ziga xos sirt maydonlariga ega bo'lib, shu bilan yorug'likni singdirish samaradorligini oshiradi. Shu bilan birga, 12 soat ichida atalaning yorug'lik o'tkazuvchanligining kichik o'zgarishi, quyida keltirilgan rasmda ko'rsatilganidek, statik jarayon davomida atala yaxshi dispersiya barqarorligiga ega ekanligini ko'rsatadi.

4. Zeta potensialining xarakteristikasi
Zeta potentsiali elektrokinetik potentsial yoki elektromotor kuch sifatida ham tanilgan Shear tekisligining potentsialiga ishora qiladi va kolloid dispersiyalarning barqarorligini tavsiflovchi muhim ko'rsatkichdir. Molekulalar yoki dispers zarrachalar qanchalik kichik bo'lsa, Zeta potentsialining mutlaq qiymati (ijobiy yoki manfiy) shunchalik yuqori bo'ladi va tizim shunchalik barqaror bo'ladi, ya'ni eritma yoki dispersiya agregatsiyaga qarshilik ko'rsatishi mumkin. Aksincha, Zeta potentsiali (ijobiy yoki salbiy) qanchalik past bo'lsa, u shunchalik ko'p koagulyatsiyaga yoki agregatsiyaga moyil bo'ladi, ya'ni tortishish qaytarilishdan oshib ketadi, dispersiya buziladi va koagulyatsiya yoki agregatsiya sodir bo'ladi.

Batareya shlamining dispersiyasini tavsiflash usuli
1. Noziklik
Noziklik batareya shlamining muhim ishlash ko'rsatkichidir, bu atala zarrachalarining hajmi va tarqalishi kabi ma'lumotlarni aks ettirishi mumkin. Noziklik qiymati atala tarkibidagi zarrachalar tarqalib ketganmi yoki aglomeratlar deaglomeratsiyalanganmi yoki yo'qligini tushunish uchun ishlatilishi mumkin.

2. Membrananing empedansi
Lityum batareyali atala - bu elektrod faol moddalari va o'tkazuvchan moddalarni biriktiruvchi eritmada tarqatish natijasida hosil bo'lgan qattiq-suyuq aralash tizim. To'rt probli membrana empedansi sinovi printsipiga ko'ra, atala membrana empedansi sinovdan o'tkaziladi. Sut o'tkazuvchi agentning ataladagi tarqalish holati, atalaning dispersiya ta'sirini baholash uchun qarshilik orqali miqdoriy jihatdan tahlil qilinishi mumkin. Maxsus sinov jarayoni: izolyatsion plyonkada atala bir tekisda qoplanishi uchun kino aplikatoridan foydalaning, so'ngra uni qizdiring va quriting, quritgandan keyin qoplamaning qalinligini o'lchang, namunani kesib oling va o'lcham cheksiz talabga javob beradi. Nihoyat, elektrod membranasi empedansini o'lchash va qalinligi asosida qarshilikni hisoblash uchun to'rtta probdan foydalaning.
3. Skanerli elektron mikroskop/energiya spektr tahlili/krioelektron mikroskop
Skanerli elektron mikroskop (SEM) batareya atalasining morfologiyasini bevosita kuzatish va har bir komponentning tarqalishini tahlil qilish uchun energiya spektrini tahlil qilish (EDS) bilan hamkorlik qilish uchun ishlatilishi mumkin. Biroq, namunalarni tayyorlashda, bu jarayon davomida atala quritilishi o'z tarkibiy qismlarining qayta taqsimlanishiga olib kelishi mumkin. Krio-elektron mikroskopiya (Cryo-SEM) atala tarkibiy qismlarining asl tarqalish holatini saqlab turishi mumkin, shuning uchun u yaqinda atala xususiyatlarini tahlil qilishda qo'llanila boshlandi.
4. Elektrodli kompyuter tomografiyasi
Elektrodli kompyuter tomografiyasi elektroddagi zarrachalarning dispersiya holatini bevosita kuzatishi mumkin. Quyidagi rasmda ko'rsatilganidek, a-rasmdagi elektrodda yig'ilgan yirik zarrachalar ko'proq, b-rasmdagi elektroddagi aglomeratsiyalangan zarrachalar sezilarli darajada kamayadi va v-rasmdagi elektrodda aglomeratsiyalangan yirik zarrachalar deyarli yo'q.

5. Lazerli diffraktsiyani o'lchash texnologiyasi
Lazer diffraktsiyasini o'lchash texnologiyasi zarrachalar hajmi va tarqalishini olish uchun Fresnel tarqalishi nazariyasi va Fraunhofer nazariyasini qo'llaydi. Ushbu texnologiyaga asoslangan lazer zarrachalari o'lchami analizatori yuqori o'lchov aniqligi, yaxshi takrorlanishi va qisqa o'lchash vaqtiga ega. U akkumulyator zavodlarida batareyalardagi atala zarrachalarining hajmini sinash uchun keng qo'llanilgan.
6. Elektrokimyoviy impedans spektroskopiya tahlil usuli
Masalan, Vang va boshqalar. suyuq atalaning impedans spektrini to'g'ridan-to'g'ri tahlil qilish uchun elektrokimyoviy impedans spektroskopiya tahlil usuli (EIS) dan foydalangan va turli zarrachalar konsentratsiyasida atalaning elektrokimyoviy xususiyatlarini olgan. Empedans spektrini o'rnatish natijalari orqali parametr ekvivalent sxemasi modeliga asoslangan elektrod shlamining ichki zarrachalarini taqsimlash strukturasini baholash usuli o'rnatildi, bu ichki bir xil bo'lmagan strukturani onlayn o'lchash va onlayn baholash uchun yangi g'oyani taqdim etdi. litiy-ion batareyasi atalasining. EIS test printsipi rasmda ko'rsatilgan.

Atlama turg'unligini va tarqalish qobiliyatini tavsiflash usullari
1. Reometr
(1) Viskoelastiklik testi
The viscoelastic characteristics of the slurry are characterized by the relative valuesof the storage modulus (G′) and the loss modulus (G″). The storage modulus G′, also known as the elastic modulus, represents the capacity stored when the slurry undergoes reversible elastic deformation and is a measure of the elastic deformation of the slurry. The loss modulus G″, also known as the viscous modulus, represents the energy consumed when the slurry undergoes irreversible deformation and is a measure of the viscous deformation of the slurry. In the frequency scan, based on the relative size of G′and G″and evaluating the sensitivity of G′to the angular frequency, it is possible to reflect whether the slurry is in a fluid state or a solid-like state. In the low-frequency range, G′>G" va farq qanchalik katta bo'lsa, atala barqarorligi shunchalik yaxshi bo'ladi. Quyidagi rasmda ko'rsatilganidek, tabiiy grafit atalasining barqarorligi sintetik grafit shlamiga qaraganda yaxshiroq.

(2) Kesish tezligi bilan yopishqoqlikning o'zgarishi
Atlamaning yopishqoqligi odatda kesish tezligi bilan o'zgaradi. Kesishda yupqalash harakati mavjud bo'lganda, atala ichida yumshoq aglomeratlar mavjud bo'lib, ular kesish ta'sirida osongina yo'q qilinadi. Aksincha, kesish qalinlashuvining mavjudligi odatda atalada qattiq agregatlangan zarralar mavjudligini ko'rsatadi. Umuman olganda, kesish tezligi tezroq bo'lgan shlamlar, kesish kuchi bilan bog'lovchining yo'q qilinishini e'tiborsiz qoldirib, yaxshi tarqalish qobiliyatiga ega. Quyidagi rasmda ko'rsatilganidek, ichi bo'sh doira bilan ifodalangan atala boshqa ikkita bulamalga qaraganda yaxshiroq dispersiyaga ega.

(3) Hosildorlik stress testi
Reologiyada oqish kuchlanishi namunada qaytarilmas plastik deformatsiya birinchi marta kuzatiladigan qo'llaniladigan kuchlanish sifatida aniqlanadi. Nazariy jihatdan, oqim kuchlanishi oqimni boshlash uchun zarur bo'lgan minimal stressdir. Hosildorlikni tahlil qilish barcha murakkab tuzilmali suyuqliklar uchun muhimdir. Yaroqlilik muddati va cho'kindi yoki fazalarni ajratishga qarshi barqarorlik kabi mahsulotning ishlashini yaxshiroq tushunishga yordam beradi. Hosildorlikni aniqlash uchun turli xil reologik usullar mavjud. Quyidagi rasmda kesish oqimini pasaytirish usulidan foydalangan holda rentabellik stressi tahlili ko'rsatilgan. Sinov natijalaridan ko'rinib turibdiki, o'rtacha siljish tezligida siljish tezligi pasayganda kesish kuchlanishi kamayadi. Biroq, siljish tezligi yanada kamaytirilganda, kuchlanish egri chizig'i barqaror darajaga etadi va tezlikdan mustaqil bo'ladi. Ushbu barqaror kuchlanish qiymati hosil nuqtasi deb ataladi. Shu bilan birga, o'lchangan "ko'rinadigan yopishqoqlik" egri chizig'i cheksiz bo'ladi va qiyalik -1 bo'lganda siljish tezligi bilan chiziqli bog'liqlikka ega.

Sintetik grafit kattaroq zarracha hajmi va tartibsiz zarracha shakliga ega bo'lganligi sababli, atala past rentabellikdagi stressni va zaifroq tarmoq tuzilishini namoyish etadi. Shuning uchun, bu sintetik grafit atala namunasi cho'kindi va fazalarni ajratishga ko'proq moyil bo'ladi. Atlama cho'kishi elektrodda faol materiallarning notekis taqsimlanishiga olib kelishi mumkin va shu bilan batareyaning ishlashini pasaytiradi.
(4) tiksotropiya
Qoplagandan so'ng, akkumulyator eritmasi oqim kollektoridagi tortishish va sirt tarangligi ta'sirida tekislanadi. Past kesish tezligi oralig'ida, qoplamadan oldin yopishqoqlik asta-sekin yuqori viskoziteye qaytadi, deb umid qilinadi. Yuqori yopishqoqlikka qaytishdan oldin, atalaning yopishqoqligi hali ham nisbatan past, tekislash oson va qoplama yuzasi silliq va qalinligida bir xil bo'ladi. Qayta tiklash muddati juda uzoq yoki juda qisqa bo'lmasligi kerak. Qayta tiklash muddati juda uzoq bo'lsa, tekislash jarayonida atala viskozitesi juda past bo'ladi va quyruqga ega bo'lish oson yoki pastki chetining qalinligi yuqori qoplamaning qalinligidan yuqori. Vaqt juda qisqa bo'lsa, atala tekislash uchun vaqt topolmaydi.
2. Atlama qarshiligini o'lchagich
Atlama qarshiligi parametri atala formulasi, o'tkazuvchi vositaning turi va tarkibi, biriktiruvchining turi va tarkibi va boshqalar bilan sezilarli bog'liqlikka ega. Atlama aralashtirib, ma'lum vaqt turishga qo'yilgandan so'ng, jel cho'kishi mumkin. sodir bo'ladi va qarshilik qiymati ham turli darajadagi o'zgarishlarni ko'rsatadi. Shuning uchun, atala qarshiligi atala elektr xususiyatlarining bir xilligi va barqarorligini tavsiflash usuli sifatida ishlatilishi mumkin.
Sinov usuli:ma'lum hajmdagi atala (taxminan 80 ml) o'lchov stakaniga soling, toza elektrod qalamini joylashtiring, dasturiy ta'minotni ishga tushiring, vaqt o'tishi bilan uch juft elektrodda atala qarshiligining o'zgarishini sinab ko'ring va uni hujjatga saqlang.
Sinov parametrlari:qarshilik, harorat, vaqt
Hisoblash formulasi:Qarshilik (Ω*sm):Se=U/I * S/L
Xususiyatlari:
1. Kuchlanish va oqim liniyalarini ajratib oling, indüktansning kuchlanishni o'lchashga ta'sirini yo'q qiling va qarshilikni aniqlash aniqligini yaxshilang.
2. 10 mm diametrli disk elektrodi namuna bilan nisbatan katta aloqa maydonini ta'minlaydi va sinov xatosini kamaytiradi.
3. Vaqt o'tishi bilan atalaning vertikal yo'nalishi bo'yicha uchta pozitsiyada qarshilik o'zgarishi real vaqtda kuzatilishi mumkin.
Qarshilikni o'lchash diapazoni:2,5 Ō * sm ~ 50 MŌ * sm
Qarshilikni o'lchash aniqligi:±0.5%